Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.73 - 2.87 cP | 2.73 - 2.87 cP | 98% H2SO4 |
UBE 7024B Nylon 6/12 Copolymer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |