Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.67 cP | 2.67 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer) Geon® 138 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy savings and the ability to work with heat sensitive substrates. The.. |
|||
Relative Viscosity | 2.67 - 2.73 cP | 2.67 - 2.73 cP | 1% in 96% H2SO4; ISO 307 |
Azoty Tarnow™ Alphalon™ 27D Nylon 6 A bright polyamide 6 grade of low viscosity suited for the production of compounds.Information provided by ATT Polymers™ |