Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.51 cP | 2.51 cP | |
Formosa Plastics Formolon® 690 PVC Homopolymer General Purpose Grade Resin F690 is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, thi.. |