Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.12 cP | 2.12 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 170 Series Adept E 49 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Adept E49 is a low molecular weight homopolymer dispersion resins intended for use in variety of plastisol applications and processes. It reduces scrap rates and manufacturing costs by extend.. |
|||
Relative Viscosity | 2.12 cP | 2.12 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 120 Series 124A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 124A is low molecular weight resin providing lower gelation and faster fusion characteristics. It provideds good chemical foamability for producing medium to high density foams. It gives good.. |
|||
Relative Viscosity | 2.12 cP | 2.12 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 210 Series 215 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 215 is a low molecular weight particle size homopolymer blending resin intended for use in plastisol formulations. It improves air release performance resulting in reduced scrap rates. It dec.. |