Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 1.8 - 1.9 cP | 1.8 - 1.9 cP | LCL-PR21 |
Intercontinental Polymers 553 PBT Polymer Type - Elastomer, Polyester Pellets Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers. |