Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 70 g/10 min

@Load 2.16 kg,
Temperature 330 °C
70 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT1141 PC
XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 70 g/10 min

@Load 2.16 kg,
Temperature 330 °C
70 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT1141 PC (Asia Pacific)
XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 70 g/10 min

@Load 2.16 kg,
Temperature 330 °C
70 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT1141 PC (Europe-Africa-Middle East)
XHT1141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 70 g/10 min

@Load 5.00 kg,
Temperature 265 °C
70 g/10 min

@Load 11.0 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..