Physical Properties Metric English Comments
Melt Index of Compound 33 g/10 min

@Load 10.0 kg,
Temperature 220 °C
33 g/10 min

@Load 22.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycolac® FXS600AR ABS (Europe-Africa-Middle East)
Visual Ares effect Cycolac ABS material with excellent flow properties.
Melt Index of Compound 33 g/10 min

@Load 5.00 kg,
Temperature 300 °C
33 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East)
Melt Index of Compound 33 g/10 min

@Load 1.20 kg,
Temperature 300 °C
33 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East)
XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C