Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 32 g/10 min @Load 5.00 kg, Temperature 250 °C |
32 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |