Physical Properties Metric English Comments
Melt Density 0.956 g/cc
0.0345 lb/in³
Melt density
Americas Styrenics Styron® XL-8028 High Impact Polystyrene  (discontinued **)
STYRON® XL-8028 high impact polystyrene is designed for VCR cassettes, toys, small appliances, telephones, housewares, tool items, computer consoles and bodies for computer cartridges. It offers hi..