Polymer Property : Melt Density = 0.914 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Density 0.914 g/cc
0.0330 lb/in³
Melt density
Dow Tyril® 125 SAN
Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov..