Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Carbon Dioxide Transmission 59.0 cc-mm/m²-24hr-atm
150 cc-mil/100 in²-24hr-atm
ASTM D1434
Eastman Eastar A150 Copolyester, Film
Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan..