Physical Properties | Metric | English | Comments |
---|---|---|---|
Carbon Dioxide Transmission | 16.7 cc-mm/m²-24hr-atm | 42.4 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman Eastobond 19411 Copolyester, Film Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so.. |
|||
Carbon Dioxide Transmission | 16.7 cc-mm/m²-24hr-atm | 42.4 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman Eastobond 19412 Copolyester, Film Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob.. |