Physical Properties | Metric | English | Comments |
---|---|---|---|
Carbon Dioxide Transmission | 87.0 cc-mm/m²-24hr-atm | 221 cc-mil/100 in²-24hr-atm | ASTM D1434 |
Eastman Sahara Film Sahara Films are developed for use in applications where increased temperature resistance is desired.Applications/UsesHigh temperature printable films |