Polymer Property : Moisture Vapor Transmission = 56.0 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 55.0 - 56.0 cc-mm/m²-24hr-atm
140 - 142 cc-mil/100 in²-24hr-atm
Average value: 55.3 cc-mm/m²-24hr-atm Grade Count:3
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..