Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 2.00 cc-mm/m²-24hr-atm | 5.08 cc-mil/100 in²-24hr-atm | Exxon Method - Extrusion coating on a 8.9 cm coating line at 30 cm/s and melt temp. of 329°C |
ExxonMobil Escorene® LD-203 LDPE Extrusion Coating for Milk Cartons, High Speed
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low density polyethylene resin with excellent adhesion, drawability and heat sealability. LD-203 also exhibits excellent barrier properties and g.. |