Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 1.46 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
3.71 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
g-mm/m²-day; based on film thickness; ASTM E96; ASTM E96 |
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |