Polymer Property : Moisture Vapor Transmission = 2.90 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.300 - 2.90 cc-mm/m²-24hr-atm
0.762 - 7.37 cc-mil/100 in²-24hr-atm
Average value: 1.22 cc-mm/m²-24hr-atm Grade Count:5
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..