Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.730 cc-mm/m²-24hr-atm | 1.85 cc-mil/100 in²-24hr-atm | Tested per ASTM F372 at 100°F, 90% RH. |
DuPont Teijin Films Mylar® 800C Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Melinex® 800C is a clear, one side corona treated polyester film suitable for flexible packaging, printing and laminations. Melinex® 800C is a polyester.. |
|||
Moisture Vapor Transmission | 0.730 cc-mm/m²-24hr-atm | 1.85 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |