Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 1.74 cc-mm/m²-24hr-atm | 4.42 cc-mil/100 in²-24hr-atm | 40°C- 90% RH; based on 30 µm layer |
Noltex Soarnol® ST110 Ethylene Vinyl Alcohol Copolymer Modified DC3203; improved flex crack resistance and thermoformability. Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of n.. |