Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.570 cc-mm/m²-24hr-atm | 1.45 cc-mil/100 in²-24hr-atm | g.mm/m2.day; 37.8°C (100°F) and 90% relative humidity (ASTM F 1249) |
Advanced Elastomer Systems Trefsin® 3201-65 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
Moisture Vapor Transmission | 0.570 cc-mm/m²-24hr-atm | 1.45 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack.. |
|||
Moisture Vapor Transmission | 0.570 cc-mm/m²-24hr-atm | 1.45 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OL12 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL12 (formerly known as XM963A) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sea.. |
|||
Moisture Vapor Transmission | 0.570 cc-mm/m²-24hr-atm | 1.45 cc-mil/100 in²-24hr-atm | g.mm/m2.day; 37.8°C (100°F) and 90% relative humidity (ASTM F 1249) |
Advanced Elastomer Systems Trefsin® 3101-65 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |