Physical Properties Metric English Comments
Moisture Vapor Transmission 1.42 cc-mm/m²-24hr-atm

@Thickness 0.0254 mm
3.61 cc-mil/100 in²-24hr-atm

@Thickness 0.00100 in
g-mm/m²-day; based on film thickness; ASTM E96; ASTM E96
DuPont Elvax® 3165SB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..