Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.510 cc-mm/m²-24hr-atm | 1.30 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Moisture Vapor Transmission | 0.510 cc-mm/m²-24hr-atm | 1.30 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Moisture Vapor Transmission | 0.510 cc-mm/m²-24hr-atm | 1.30 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® AFG Polyolefin Shrink Packaging Film, Anti-fog, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially-oriented, heat-shrinkable, anti-fog polyolefin film. The film has excellent gloss, stretch recovery, toughness and tear resista.. |