Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 1.10 cc-mm/m²-24hr-atm | 2.79 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Moisture Vapor Transmission | 1.10 cc-mm/m²-24hr-atm | 2.79 cc-mil/100 in²-24hr-atm | ASTM 1249 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |