Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.394 cc-mm/m²-24hr-atm | 1.00 cc-mil/100 in²-24hr-atm | ASTM E96 |
Total PPR 8650 Polypropylene, Random Copolymer ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for orie.. |