Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.590 - 0.940 cc-mm/m²-24hr-atm | 1.50 - 2.39 cc-mil/100 in²-24hr-atm | Average value: 0.789 cc-mm/m²-24hr-atm Grade Count:8 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |