Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.940 cc-mm/m²-24hr-atm | 2.39 cc-mil/100 in²-24hr-atm | g-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96 |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |