Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.330 cc-mm/m²-24hr-atm | 0.838 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op.. |
|||
Moisture Vapor Transmission | 0.330 cc-mm/m²-24hr-atm | 0.838 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 150 Gauge Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo.. |