Polymer Property : Moisture Vapor Transmission = 0.406 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.160 cc-mm/m²-24hr-atm
0.406 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips HiD® 9632 HDPE Blown Film Resin  (discontinued **)
Characteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown Ideally Suited for Thin Films Production, Lower Melt Index (Higher Molecular Weight) Results in Increased Film Stre..