Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.0300 - 0.260 cc-mm/m²-24hr-atm | 0.0762 - 0.660 cc-mil/100 in²-24hr-atm | Average value: 0.163 cc-mm/m²-24hr-atm Grade Count:15 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |