Polymer Property : Moisture Vapor Transmission = 0.150 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.150 cc-mm/m²-24hr-atm
0.381 cc-mil/100 in²-24hr-atm
ASTM D1434
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer.
Moisture Vapor Transmission 0.150 cc-mm/m²-24hr-atm
0.381 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin
Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not..