Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Moisture Vapor Transmission = 0.0120 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.0120 cc-mm/m²-24hr-atm
0.0305 cc-mil/100 in²-24hr-atm
metallized barrier; 2.8 g/100in²-24hr-atm unmetallized barrier; Tested per ASTM F372 at 100°F, 90% RH.
DuPont Teijin Films Mylar® 813 Polyester Packaging Film, 48 Gauge
Data provided by DuPont Packaging Polymers.Melinex® 813 is a polyester film, pretreated on one side to provide excellent adhesion to a wide range of both solvent- and water-based inks. Melinex® 8..
Moisture Vapor Transmission 0.0120 cc-mm/m²-24hr-atm
0.0305 cc-mil/100 in²-24hr-atm
metallized barrier; 2.8 g/100in²-24hr-atm unmetallized barrier; Tested per ASTM F372 at 100°F, 90% RH.
DuPont Teijin Films Mylar® 800 Polyester Packaging Film, 48 Gauge
Data provided by DuPont Packaging Polymers.Melinex® 800 is a clear, non-pretreated base film with high gloss, low haze and excellent processability. Melinex® 800 is available in 48 gauge. Meline..