Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 6.0 hour | 6.0 hour | F50; ASTM D1963B |
ExxonMobil HDPE HD 6704.18 High Density Polyethylene Copolymer Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |
|||
ESCR 10% Igepal® | 6.0 hour @Temperature 50.0 °C |
6.0 hour @Temperature 122 °F |
F50; ASTM D1963 |
ExxonMobil HDPE HMA 014 High Density Polyethylene Resin Product Description: HMA 014 is a UV stabilized HDPE grade, characterized by excellent dimensional stability, high stiffness and high impact strength.Availability: Africa & Middle East, Asia Pacific.. |
|||
ESCR 10% Igepal® | 6.0 hour | 6.0 hour | ASTM D1693B |
ExxonMobil LLDPE LL 6201RQ Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go.. |
|||
ESCR 10% Igepal® | 6.0 hour | 6.0 hour | ASTM D1693B |
ExxonMobil LLDPE LL 6201XR Molding Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6201 series are high flow LLDPE grades, which offer unique combination of excellent processability and outstanding product properties. Parts manufactured from LL 6201 Have go.. |