Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | >= 5000 hour | >= 5000 hour | IEC 811-4-1/B, ASTM D1693-A |
Borealis Borcoat™ HE3450 Black High Density Polyethylene Top Coat for Steel Pipe Coating Borcoat HE3450 is a black, high-density polyethylene (HDPE) produced with the advanced Borstar technology, providing the material with especially well melt strength and extrudability. Also its mech.. |
|||
ESCR 10% Igepal® | >= 5000 hour | >= 5000 hour | IEC 811-4-1/B, ASTM D1693-A |
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating Borcoat HE3453 is a natural and colorable high density polyethylene produced with the Borstar technology in similar conditions as the black ready made top coat Borcoat HE3450. Borcoat HE3453 is rec.. |
|||
ESCR 10% Igepal® | >= 5000 hour | >= 5000 hour | ASTM D1693-A |
Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor.. |