Polymer Property : ESCR 10% Igepal® = 25 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 10% Igepal® 25 hour
25 hour
Condition A, F50; ASTM D-1693
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE
High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren..