Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 24 hour | 24 hour | ASTM D1693 |
ExxonMobil LL 8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
ESCR 10% Igepal® | 24 hour | 24 hour | ASTM D1693 |
ExxonMobil LLP8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |