Borealis Borecene™ RM8402 Linear Polyethylene for Rotational Molding
Borecene RM8402 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro..
ESCR 10% Igepal® >= 120 hour
>= 120 hour
ARM Method
Borealis Borecene™ RM8403 Linear Polyethylene for Rotational Molding
Borecene RM8403 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro..