Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 110 hour @Temperature 50.0 °C |
110 hour @Temperature 122 °F |
F<sub>50</sub>; Condition A, From compression molded specimens; ASTM D1693 |
NOVA Chemicals Novapol® TR-0338-UI Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |
|||
ESCR 10% Igepal® | 110 hour @Temperature 50.0 °C |
110 hour @Temperature 122 °F |
F<sub>50</sub>; Condition A, From compression molded specimens; ASTM D1693 |
NOVA Chemicals Novapol® TR-0338-UIG Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |