Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | >= 920 hour | >= 920 hour | ASTM D-1693 |
Bapolene® 5010H High Density Polyethylene This resin is a high molecular weight, high density copolymer polyethylene resin. Product exhibits superior impact strength and ESCR. Resin contains a process stabilizer and complies with FDA 21 C.. |