Polymer Property : ESCR 100% Igepal® = 80 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 100% Igepal® 80 hour

@Temperature 50.0 °C
80 hour

@Temperature 122 °F
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol..
ESCR 100% Igepal® 80 hour
80 hour
ASTM D1693 Condition B
ExxonMobil Paxon™ AA50-002 Blow Molding Resin  (discontinued **)
AA50-002 is a blow molding grade high density polyethylene. This resin has excellent stress crack resistance combined with high impact strength, rigidity, and melt strength.Information provided by ..