Polymer Property : ESCR 100% Igepal® = 750 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 100% Igepal® >= 750 hour
>= 750 hour
ASTM D1693
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene
MDPE Copolymer with UV8 stabilizer, available as black powder.Recommended for rotomolding. Used for manufacture of septic tanks and garbage bins. Recommended for use in combination with ROTOFOAM B..