Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 700 hour | 700 hour | Condition A, F50; ASTM D-1693 |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |