Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : ESCR 100% Igepal® = 7.0 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
ESCR 100% Igepal® 7.0 hour
7.0 hour
F50; ASTM D1693B
SABIC M40053S High Density Polyethylene for Injection Molding
Product Description: M40053S is a UV stabilized high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to pro..