Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 33 hour | 33 hour | F<sub>50</sub>; ASTM D1693-B |
Petromont 1000 High Density Polyethylene Resin Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to .. |
|||
ESCR 100% Igepal® | 33 hour | 33 hour | F<sub>50</sub>; ASTM D1693-B |
Petromont 1002 High Density Polyethylene Resin Petromont HDPE 1002 is a blow moulding high-density polyethylene copolymer resin produced using the UNIPOL® Process. This multi-purpose resin can be used on intermittent and continuous extrusion bl.. |
|||
ESCR 100% Igepal® | 33 hour @Thickness 2.00 mm, Temperature 50.0 °C |
33 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem HB0454HR HDPE Blow Molding Polyethylene Copolymer HB0454HR is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454HR shows excellent processability, color, and superfi.. |