Physical Properties Metric English Comments
ESCR 100% Igepal® 25 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
25 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Braskem GF4960 HDPE Blow Molding Polyethylene Homopolymer
GF 4960 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance. It was developed for the blow-molding segment. It is used in containers for y..
ESCR 100% Igepal® 25 hour
25 hour
ASTM D1693 Condition B
ExxonMobil Paxon™ AM55-003 Blow Molding Resin  (discontinued **)
AM55-003 is a blow molding grade high density polyethylene copolymer containing an excellent antistat additive. It provides a good combination of stiffness and stress crack resistance. AM55-003 co..
ESCR 100% Igepal® 25 hour
25 hour
ASTM D1693 Condition B
ExxonMobil Paxon™ AS55-003 Blow Molding Resin  (discontinued **)
AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance.Information provided by Exx..
ESCR 100% Igepal® 25 hour
25 hour
ASTM D1693 Condition B
ExxonMobil Paxon™ AU55-003 Blow Molding Resin  (discontinued **)
AU55-003 is a blow molding grade high density polyethylene containing an excellent antistat additive, offering a good combination of stiffness and stress crack resistance. An enhanced additive pack..
ESCR 100% Igepal® 25 hour

@Temperature 50.0 °C
25 hour

@Temperature 122 °F
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene
Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con..