Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 2.0 hour @Temperature 50.0 °C |
2.0 hour @Temperature 122 °F |
F<sub>50</sub>; Molded and tested in accordance with ASTM D4976; ASTM D1693 |
Dow DMDA-8007 NT 7 High Density Polyethylene Resin DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin .. |
|||
ESCR 100% Igepal® | <= 2.0 hour @Thickness 2.00 mm, Temperature 50.0 °C |
<= 2.0 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem IA58 HDPE Injection Molding Polyethylene Copolymer IA58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good .. |
|||
ESCR 100% Igepal® | <= 2.0 hour @Thickness 2.00 mm, Temperature 50.0 °C |
<= 2.0 hour @Thickness 0.0787 in, Temperature 122 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem IB58 HDPE Injection Molding Polyethylene Copolymer IB58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good .. |