Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 16 hour @Thickness 3.00 mm, Temperature 23.0 °C |
16 hour @Thickness 0.118 in, Temperature 73.4 °F |
compression molded plaques; ASTM D1693B |
Braskem BT 003 HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles for food products, lubricating and cooking oil; toys; bottler for surface-active agents; sheets. Information provided by Braskem |