Polymer Property : Viscosity Test = 93 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 93 cm³/g
93 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® B 4235 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Viscosity Test 93 cm³/g
93 cm³/g
Viscosity number; ISO 307, 1157, 1628
Lanxess Pocan® BF 4235 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant