Polymer Property : Viscosity Test = 89 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 89 cm³/g
89 cm³/g
Reduced viscosity, K value = 60; ISO 1628-2
SolVin 260RF Polyvinyl Chloride General Purpose - Rigid
Made by suspension polymerization. APPLICATIONS Extrusion : unplasticized PVC - tubes/pipes - profile - foam - sheet, film - blow moldings Calendering : unplasticized PVC - film : high temperature p..
Viscosity Test 89 cm³/g
89 cm³/g
Reduced viscosity, K value = 60; ISO 1628-2
SolVin 560RA Copolymer of Vinyl Chloride and Vinyl Acetate
Made by suspension polymerization. APPLICATIONS Extrusion : sheets for vacuum-forming, for deformations of over 500 % Calendering : rigid sheets for deep thermoformingInformation provided by SolVin...
Viscosity Test 89 cm³/g
89 cm³/g
Viscosity number
BASF Ultradur B 4300 G6 LS High Speed BK15045 30% Glass Filled PBT