Physical Properties Metric English Comments
Viscosity Test 61 - 63 cm³/g
61 - 63 cm³/g
Ubbelhode
Iran Petrochemical (PCC) TG 621 Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, semi dullApplications: staple fiber, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co.
Viscosity Test 61 cm³/g
61 cm³/g
Limiting Viscosity Number; ISO 1628-4
Mitsubishi Xantar® 27 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 61 cm³/g
61 cm³/g
Limiting Viscosity Number; ISO 1628-4
Mitsubishi Xantar® 27 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 61 cm³/g
61 cm³/g
Limiting Viscosity Number; ISO 1628-4
Mitsubishi Xantar® 27 U Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Viscosity Test 61 cm³/g
61 cm³/g
Reduced viscosity, K value = 50; ISO 1628-2
SolVin 250SB Polyvinyl Chloride General Purpose - Rigid
Made by suspension polymerization. APPLICATIONS Injection : moldings with complex flow paths Pressing : mixed with VC-VAc copolymers for gramophone records Calendering : rigid films and sheets ; use..
Viscosity Test 61 cm³/g
61 cm³/g
Limiting Viscosity Number; ISO 1628-4
Mitsubishi Xantar® 27 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..