Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 118 - 450 cm³/g | 118 - 450 cm³/g | Average value: 190 cm³/g Grade Count:44 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |